How to choose correct silk screen mesh/polymer mesh

Date: 2013-12-27   Clicked: 3740


How to choose correct silk screen mesh/polymer mesh for silk screen printing machine


A:  Silk screen mesh choose: 

It is related below 3 different Factor

1.  Using which types of printing ink: 

   General,water based ink suitable for low density silk screen mesh(125-180mesh/inch).1 Inch=1000 mil=2.54 cm=25.4 mm

  Solvent ink printing advertising,electric will be use middle density silk screen mesh(196-420mesh/inch)

  UV ink will be choose high density silk screen mesh(355-457mesh/inch)

  General ink’s Pigment particles is very smaller,printing ink permeability will be good.Like this type ink,high density silk screen mesh aslo can permeability ok.But if printing ink with high pigment thickness,even its particles is small,but Permeability is worse.

2.  Printing products materials/surface

  If printing products with rough surface and Absorbent,it will be need more printing ink to get best printing ink cover rate,will be choose lower density silk screen mesh

  Printing products surface very smooth,it needs printing ink will be less,then should be choose high density silk screen mesh.

3.  Silk screen mesh will be match with original photoshop or Adobe illustrator file image

Choosing silk screen mesh will be enough to cover image.scilicet the smallest image area has enough silk screen mesh brace.One silk screen meesh printed the smallest line width should be equal mesh hole and mesh diameter plus silk screen weaving 7% expansion. 

For example:silk screen mesh: 180 mesh/inch, mesh hole: 23μm,silk 30μm,after printed smallest line width= 23+30+(23+30)*7%≈57μm. It means this silk screen mesh only can printed image line is 57μm. Only one formula the silk screen mesh can be complete printed small line width=√2*(1+ mesh*hole size)÷mesh)。

 

B: Choosing silk size: 

   It is related 2 different factor: Silk screen mesh Tensile Strength and photosop/Adobe illustrator file image size.


When silk screen mesh the same,silk bigger,its tensile strength,wearable and Corrosion resistance will be stronger,thickness also will be bigger but hole will be smaller.

When Photoshop/Adobe illustrator image size 2 twice of silk,AM/FM maybe on the silk,high light FM/AM will be loss

When FM/AM 3 twice of silk,any parts FM/AM will be get enough support,FM/AM will be get enough hole area.



C. Attention questions of choosing silk screen mesh

Weaving Uniform or not    

Silk mesh size uniform or not

Silk screen mesh cost

Moire



Related Posts
Next Article:different of closed ink cup system pad printer and open ink cup system pad printing machine
Prev Article:How to make silicon pad for pad printing

Copyright © Dongguan Hoystar Printing Machinery Co., Ltd. All Right Reserved. 51LA

Add:No.2,Zhenglong 2nd Road,Hengzeng Street,ChanganTown,Dongguan city,Guangdong province China   

Tel : +86-769-85377425   Fax : +86-769-82926182

Screen printing machine | Pad printing machine | Infrared Drying Machine | UV Curing Machine | Hot Stamping Machine | Heattransfer Machine | Uv-exposure-machine

Rotate screen printing machine | Flat bed screen printerCylindrical screen printer | Flame treatment equipment |Screen pringer | Automatic screen printing machine

Socks screen printer | Mini pad printing machine | Ruler screen printing machine | Mini screen printer supplier | Screen printing conveyor dryers | T-Shirt Printing Equipment

FacebookFacebook    YoutubeYoutube    Twitter Twitter     GoogleGoogle    ArabicArabic   SpanishSpanish   PortuguesePortuguese   RussianRussian    FrenchFrench    TurkishTurkish    GermanGerman    ItalianItalian

 
在线客服乐语
Live Chat